• Fengfan Aluminum Anodizing Chemicals Liquid Sealing Agent For Color Dyes Anodized Seal 147
  • Fengfan Aluminum Anodizing Chemicals Liquid Sealing Agent For Color Dyes Anodized Seal 147

Fengfan Aluminum Anodizing Chemicals Liquid Sealing Agent For Color Dyes Anodized Seal 147

Nickel acetate liquid sealing agent for dyed anodized aluminum. It rinses clean, leaves no film before rinsing and rarely bleaches color.
  • Fengfan Aluminum Anodizing Chemicals Liquid Sealing Agent For Color Dyes Anodized Seal 147

Description

Product Overview

Phoenix Seal 147 is a nickel acetate sealing agent in liquid form, made for anodized aluminum that has been colored before sealing. It is a dark green, weakly acidic liquid that goes into the sealing tank ready to dilute, and it is used at the end of the line, after dyeing and before drying. At working temperature the nickel acetate reacts with the open pores of the anodic film and closes them around the dye already sitting in the pore, so moisture, cleaning agents and handling soils stay out and the color stays in. The sealed layer also adds a little surface hardness and improves resistance to the light abrasion that parts meet in packing and installation.

What separates this sealer from a general-purpose one is what happens when the rack leaves the tank. No film forms before the rinse, the parts rinse clean, and bleaching of dyed anodized aluminum is rare when temperature, time and pH are held inside the working window. On a decorative part that shows up as brightness that survives, a smooth hand rather than a chalky one, and color contrast between masked areas that stays where the designer put it.

It works at both ends of the scale. A plant running an aluminum anodizing service on panels, signage or trim can charge it into an existing sealing tank without rebuilding the line, while a smaller shop coloring batches in an aluminum anodizing kit setup runs the same bath at the same settings. Either way it is a liquid concentrate: measure, mix, heat, and the bath is ready.

Operating Parameters

ParameterSetting
Concentration20 ~ 30 ml/L; optimum at 25 ml/L
Temperature70 ~ 100 °C; optimum at 80 ~ 95 °C
Sealing time0.5 ~ 2 min/µm; optimum at 1 min/µm
pH5.0 ~ 6.0; optimum at 5.0 ~ 5.5
Air stirringWeak air stirring suggested
Circulation filtrationSuggested, with acid- and heat-resistant filter media
Tank materialStainless steel SUS304 or SUS316
Base chemistryNickel acetate
AppearanceDark green acidic liquid

Dye Retention and Color Stability

  • The dye stays in the pore. Sealing closes the pore around the dye instead of flushing it out, and bleaching of dyed anodized aluminum is rare when the bath is held inside the temperature, time and pH window.
  • Color contrast survives. On parts masked into two or more colors, the sealed anodized coating keeps the contrast between areas instead of letting the lighter shade drift toward the darker one.
  • Gloss and hand feel hold up. Sealed surfaces keep their brightness and a smooth, non-chalky hand, so decorative parts do not need a polish or a wipe-down after sealing.
  • Less mottling under raking light. Patchy tone shows up under directional light long before it shows in a photograph; a clean rinse and a stable bath keep that patchiness off the finished anodized metal.
  • Deep shades are the honest test. Black anodized aluminum and dark bronze show any tone shift immediately, which is why color-critical work is sealed in a bath that rinses clean and rarely bleeds dye.
  • Protection that lasts past the rack. The sealed layer resists the light abrasion of handling, packing and installation, and keeps the surface from dulling in service.

Line Integration and Automatic Production

On a busy line, a sealer is judged by what it does to the flow of parts as much as by the finish. Because no film forms before rinsing, a rack can leave the sealing tank, go through the rinse and on to drying without a wiping station in between. That takes a manual step out of the route, keeps the rinse water cleaner for longer, and shortens the time a rack spends between sealing and packing, which is where the throughput gain shows up on an automatic or semi-automatic installation.

The bath is undemanding to hold. Weak air stirring is all it asks for, so there is no need for vigorous agitation to keep temperature and concentration even across the tank. Running the bath through a filter loop keeps particles out of the film; specks on a sealed surface almost always come from the bath rather than from the sealer. And because the working window sits inside equipment most shops already run, putting this sealer into an existing aluminum anodizing line is usually a matter of charging the tank rather than rebuilding it.

It scales down as cleanly as it scales up. A full line with automatic transfer runs it as the final wet stage of the aluminum anodizing process before drying; a workshop coloring a few racks a week runs the identical bath in a single tank, at the same concentration and the same dwell. Because the sealing stage stops being a variable, color drift between batches falls, and the rack that comes off on Friday matches the one that came off on Monday.

Sealing Procedure and Bath Care

  1. Flush and charge. Rinse the sealing tank clean, fill to working volume, measure in the sealer and stir. It is a liquid concentrate, so it disperses in a few minutes and there is no powder to dissolve or dust at the tank.
  2. Heat before the first rack. Bring the bath to working temperature before any parts go in. A bath still climbing through the range seals unevenly across a rack and leaves the first load of the shift with a different result from the last.
  3. Hold the pH inside the window. Check pH with a meter at the start of the run and again after a long shift. Drift is the usual reason a bath that sealed well last week starts pulling color out of the work.
  4. Stir gently and filter continuously. Weak air movement evens out temperature and concentration across the tank; keep the filter loop running through the shift so the bath stays clear.
  5. Time to film thickness, not to the clock. A dwell that suits a thin decorative film on an anodized metal part is too short for a thick architectural one. Work from the micron figure, write the time on the route card, and keep it the same for repeat orders.
  6. Rinse as soon as the rack leaves the tank. Move parts straight to the rinse and rinse until the water runs clear, then dry as usual. In an aluminum anodizing process the rinse is often the step where a good seal is either kept or lost.
  7. Log and top up. Record concentration, pH, temperature and running hours, and top up on drag-out and analysis rather than by guess. A written log is what turns a good first batch into a repeatable process.

Typical Applications

  • Architectural panels and facade trim. Colored sheet and extrusions for cladding, louvers and window trim, where panels from different batches still have to read as one facade; for a shop running an aluminum anodizing service, sealing is what holds that consistency together.
  • Signage and display hardware. Outdoor signs and display frames that meet sun, humidity and regular cleaning; sealing cuts water spotting and keeps lettering and color contrast legible.
  • Consumer electronics and appliance trim. Bezels, buttons, camera rings and decorative trim in colored anodized parts, where brightness and a smooth hand matter more than film thickness and no post-seal wiping keeps handling marks off.
  • Black and deep-shade work. Black anodized aluminum and dark bronze parts, where any tone shift shows immediately, run in the same bath and at the same dwell as light colors.
  • Job shops and small batches. A workshop running a compact aluminum anodizing kit, or a job shop coloring a few racks a week, uses one shared sealing bath without one color bleeding into the next order.
  • Parts cleaned after finishing. Sealing is the last wet step in the aluminum anodizing process, and on parts that will be wiped with solvent or washed before assembly the sealed anodized metal keeps cleaning from dulling it.

Batch Testing and Quality Control

  1. Formulation held constant. Fengfan has supplied surface-finishing chemistry to plants running an aluminum anodizing service since 1984, and this sealer is made to a fixed specification rather than adjusted from batch to batch, so a drum bought this year behaves like the drum a customer validated last year.
  2. Incoming materials checked first. Raw materials are checked against specification before they are charged to a batch; a lot that does not meet it does not go in.
  3. A real working bath, not a shortcut. Sample panels are sealed in a bath run at the same concentration, temperature and pH a customer will use, so the test reflects production rather than a laboratory ideal.
  4. Rinse behavior and residue inspected. Sealed panels are rinsed and examined for what stays on the surface after drying, which is the difference between an anodized coating that can go straight to packing and one that needs wiping.
  5. Dye stability compared with a reference. Dyed panels are sealed and checked against a retained reference shade, so a slow drift in color is caught before it reaches a customer's inspection bench.
  6. Kit and tank compatibility checked. Many customers seal in a standard aluminum anodizing kit or a simple tank setup rather than a bespoke line, so the bath is also run against those configurations.
  7. Batch number travels with the goods. Every batch is recorded, and its batch number goes on the paperwork, so a question about a specific delivery can be traced back to its production record.

Ordering and Delivery

TermDetail
Pack for this sealer25 kg plastic drum
Other pack options10 kg/box; 25 kg or 50 kg/bag; 20 kg, 25 kg, 30 kg or 200 kg/drum; 1,000 kg/IBC drum
Minimum order quantityVaries by chemical; confirmed with our sales team per order
Lead time2 weeks
Payment100% T/T in advance
ShippingPer the terms agreed in the current contract
WarrantyInspection certificate issued after delivery stating the batch number and warranty period

Design and Structural Benefits for Aluminum Anodizing Lines

Fengfan's sealing agent is built around a robust nickel acetate system, so it can be integrated into conventional aluminum anodizing kits and finishing tanks made from SUS304 or SUS316 stainless steel. The formulation is designed to work with existing anodizing equipment, which helps keep retrofit work to a minimum. Its acidic pH and dark green color make the bath easier to monitor and control, supporting safer, more precise operation. The product is supplied in 25 kg plastic drums for bulk industrial use, making storage and handling practical for anodized aluminum production lines.

Performance, Usability, and Industrial Value

The concentrated formula and the recommended immersion time deliver consistent improvements in color retention and surface gloss. Because the agent rinses easily, it helps shorten production cycles by reducing cleaning downtime and preventing residue buildup, which supports higher line throughput. When process parameters are tightly controlled, it also lowers the risk of dye bleaching and helps maintain the long-term durability of anodized aluminum finishes. That reliability gives manufacturers greater confidence in quality assurance for their anodizing process and in the color results end users see. In use, SEAL-147 fits color finishing of decorative panels for architectural decoration, signage, and consumer appliances, where anodized aluminum surfaces carry colored dyes; suitability for a specific dye and line setup should be confirmed before production.

Technical Support & Model Matching

Choosing the right match is where most sourcing decisions stall. As a trading supplier, we keep one point of contact from first enquiry to after-sales: tell us what you are making and the conditions you work under, and we shortlist the closest matches from our supplier network, compare specifications and arrange samples before you commit to a bulk order. If something does not behave as expected, we work with the supplying partner on the cause and a practical fix, and stay with the case until it is settled. Email, WeChat or WhatsApp enquiries get a reply within 24 hours.

FAQ

What does the sealing agent look like?

It is a dark green, weakly acidic liquid supplied ready to dilute, with no powder to dissolve and no separate make-up step. The color is useful at the tank: operators can see the bath level and watch the wet film on a rack as it comes out, so coverage is obvious before the part reaches the rinse.

What concentration should the bath be run at?

Mix at 25 ml/L as the working figure and stay inside 20 ~ 30 ml/L. That is the practical setting for most color work on anodized metal; the range gives you room to move without using extra chemical for no gain. If your film is unusually thick or your dye load is heavy, agree the starting point with us before the first production rack, because the bath is easier to adjust before the shift than during it.

At what temperature and for how long should parts be sealed?

Run between 70 °C and 100 °C, with 80 ~ 95 °C giving the most consistent result on dyed work. Time is set by the oxide rather than by the clock, so in an aluminum anodizing process the dwell scales with film thickness: 0.5 ~ 2 minutes per micron, with about 1 minute per micron as the standard. A 10 microns decorative film therefore needs roughly 10 minutes in the tank. Hold both figures together, since a long dwell at the top of the range costs capacity without improving the seal.

Will it damage or fade dyed colors?

Bleaching is rare when the bath is held inside the recommended temperature, time and pH window, and that is the main reason this sealer is chosen for color work. Deep shades such as black anodized aluminum are the honest test, because if a bath is going to pull dye out, it shows there first. Keep the rinse clean and the bath filtered, check pH before the run rather than after, and the color that leaves the dye tank is the color that ships.

Can it be used on alodine coated parts?

No. This is a sealing agent for dyed anodic films, while an alodine chromate conversion coating is a different surface that follows its own process. Where a line runs both anodizing and conversion coating, the sealer belongs after the anodizing and dye steps only. If you are moving a part from a conversion coating route to an anodized coating route, tell us the alloy and the finish you need and we will confirm the sequence before you commit a tank.

REQUEST MORE DETAILS

Please fill out the form below and click the button to request more information about
Name
Email *
Message
Verification Code *
Click to verify