This is a brightener from the acid zinc plating chemicals family: a two-component additive for ammonium chloride zinc baths, made for shops that want a genuinely white-bright zinc layer on a flat, well-levelled surface. It goes into the bath as a pair — a small addition of component A and a much larger addition of component B — and because the two are dosed separately, a bath can be corrected in either direction without being remade.
In the line it sits where every brightener sits in the process of electroplating: after degreasing, derusting and activation, and before the rinse, neutralisation and passivation steps that follow the zinc layer. Nothing about the tank, the rectifier or the jigging has to change to run it, because the make-up is the familiar ammonium chloride and zinc chloride pair that chloride zinc shops already work with.
Because it is one of the electroplating chemicals that has to match an existing bath rather than replace it, the sensible first step is an analysis. Send us your ammonium chloride and zinc chloride figures, the pH you run at and the parts you plate, and we will tell you whether the bath is inside the working window before you buy anything.

| Parameter | Value |
|---|---|
| Product type | Two-component brightener for zinc electroplating, from the acid zinc plating chemicals range |
| Bath system | Ammonium chloride / zinc chloride |
| Ammonium chloride (NH4Cl) | 160–240 g/L |
| Zinc chloride (ZnCl2) | 35–65 g/L |
| CX-2000A | 1–1.5 ml/L |
| CX-2000B | 40 ml/L |
| pH | 5.0–6.5 |
| Temperature | 10–40 °C |
| Cathode current density | 0.5–4 A/dm² |
| Typical deposit | White-bright zinc |
Throwing power is the property that decides how the process of electroplating behaves on shaped work rather than on flat panels: it is how much of the current still reaches the inside of a recess, the bottom of a threaded hole or the back face of a folded flange. A bath with poor throwing power plates the outside of a bracket long before the inside sees any zinc, and the part passes on the face while failing in the thread. This brightener is built around high coverage ability, so the deposit keeps building in the low current density areas instead of crowding onto the edges.
The shapes where that matters are the ordinary ones: stamped and pressed parts with deep ribs, fasteners and threaded studs, tube ends, folded sheet, and wire forms where a shadow falls behind a welded joint. On work like that, more additive is not always the fix. Check jig position, part orientation and agitation first — a surface shielded from the current cannot be rescued by chemistry.
If you run small parts loose in a barrel, tumbling does much of the distribution work for you, but load weight, barrel speed and current per barrel still decide whether the inside of a nut gets coated. Run your worst-case part as a trial load before a production barrel goes over to a new brightener, and check the recesses on a sectioned sample rather than by eye.

| Product | What it covers |
| Fengfan Brightener for SZ-30B Sulfate Zinc Plating | Sulfate zinc baths, for shops plating from a sulfate rather than a chloride make-up |
| Fengfan Bright Zinc Alkaline for Rack and Barrel Plating ZN 50 | Alkaline zinc for rack and barrel work |
| Fengfan Brightener for Cyanide Free Alkaline Zinc Plating ZN-500 | Cyanide-free alkaline zinc lines |
| Fengfan Phoenix EB 204A-204B Divalent Tin Salt Electrolytic Coloring Additive | Electrolytic colouring after anodizing |
| Fengfan Phoenix Seal 149-L Middle Temperature Sealing Agent for Aluminum Anodizing | Mid-temperature sealing on anodized aluminium |
| Fengfan Phoenix Seal 149-T Medium Temperature Sealing Agent | The companion sealing grade for anodizing lines |
| Fengfan High Deposit Brightness Copper Plating FI-970 Bright Acid Copper Plating Process | Bright acid copper plating |
| Fengfan Wood Stone Concrete Nano-Protective FF-4219 | Nano-protective coating for wood, stone and concrete |
| Fengfan Nickel Purify P3 | Nickel bath purification |
| Fengfan Environmentally Friendly Chrome Mist Inhibitor FF-116 | Chrome mist suppression at the tank |
| Chemical intermediates | Intermediates for formulators and blenders who build their own baths |
CX-2000 delivers high current efficiency and an excellent coverage rate, and those two properties work together to reduce chemical consumption and improve line productivity. The practical result is a cost-effective solution for chemical intermediates suppliers, electroless nickel plating suppliers, and surfactant manufacturers operating across global supply networks.
Choosing the right match is where most sourcing decisions stall. As a trading supplier, we keep one point of contact from first enquiry to after-sales: tell us what you are making and the conditions you work under, and we shortlist the closest matches from our supplier network, compare specifications and arrange samples before you commit to a bulk order. If something does not behave as expected, we work with the supplying partner on the cause and a practical fix, and stay with the case until it is settled. Email, WeChat or WhatsApp enquiries get a reply within 24 hours.
It will if the bath is built on ammonium chloride and zinc chloride and sits inside the working window given in the specification table. Send us your current analysis — ammonium chloride, zinc chloride, pH and the temperature you run at — and we will tell you where you stand before you commit to a drum. If the bath has drifted outside the window, correct that first; a new brightener will not fix a bath that is out of balance.
Use the bath composition table as the make-up basis: ammonium chloride, zinc chloride, the two brightener components, then pH adjustment into range. For a specific tank volume, send us the litres and we will work the charge through with you. The figures scale with volume, but it is worth having someone check them before the first fill rather than after.
Look at the deposit rather than the calendar. A loss of brightness and a loss of leveling are corrected by different components, and the two rarely fall away together, so the appearance of the work tells you which side of the bath has moved. Keep an amp-hour and addition log from day one and our technical team will turn it into a working addition rate for your line.
The layer is white-bright out of the bath, which is the tone most clear and blue-white passivations are built around. Tell us which passivation system you run and we will confirm the pairing before you plate a production load — the passivation film changes the final colour you see, so the two should be checked together on your own parts.
Usually the current is not reaching the recess rather than the brightener running out. In any metal plating process the recess is the last place to receive current, so check jig position and part orientation, make sure agitation is moving solution past the surface, and confirm the current density you are actually running before touching the bath analysis. The throwing power of this brightener gives you margin, but it cannot plate a surface the current never reaches.
It comes down to the bath, not the part. If you run an ammonium chloride and zinc chloride bath, this is the one to trial. If the bath is potassium chloride or sulfate based, or if the work goes through an alkaline zinc line, one of the other brighteners in the range is the correct starting point and the related products above show which is which. Send us the bath analysis and we will point you at the right one.
The bath make-up is the same; what changes is how the work is presented and how the current is distributed across it. Run a trial on both configurations before you commit the whole line, and check the low current density areas on a sectioned part from each configuration — barrel work in particular rewards a real trial rather than an assumption.