Fengfan 896 is a white alkaline powder for cleaning metal before plating. Mixed with water at the strength the job calls for, it strips drawing oils, machine grease, handling marks and polishing residues from the surface, so the next tank meets bare metal instead of an oily film. Within the family of coating production chemicals, this is the step that quietly decides how everything after it behaves.
The product is supplied as five formulation types rather than one universal grade. Two are built for steel, two for non-ferrous metals, zinc-aluminum alloy and aluminum, and one for parts that arrive with polishing cream on them. Three work by chemical immersion; two are electrolytic, using current to shorten the cycle and reach into recesses that a still bath cannot clear.
It comes as a powder in sealed woven sacks and is dosed by weight per tank volume, which keeps freight and storage compact compared with a ready-mixed liquid. Plating shops, job shops and in-house finishing departments use it as the first tank in industrial electroplating, ahead of derusting, activation or the plating bath itself.
| Type | Concentration | Temperature | Voltage | Current | Time | Typical duty |
| A | 50 g/L | Ambient to 50 °C | - | - | 2-10 min | Chemical degreasing for steel; cleaning and rinse degreasing for machined parts |
| B | 50 g/L | Ambient to 50 °C | - | - | 2-10 min | Chemical degreasing for non-ferrous metal, zinc-aluminum alloy and aluminum |
| C | 50 g/L | 35-50 °C | 5-7 V | 2-4 A | 1-2 min | Electrolytic degreasing for steel |
| D | 20 g/L | 35-50 °C | 5-7 V | 2-4 A | 1-2 min | Electrolytic degreasing for non-ferrous metal, zinc-aluminum alloy and aluminum |
| E | 50 g/L | 40-75 °C | - | - | 1-5 min | Chemical degreasing for metal surfaces treated with polishing cream |
Three of the five types work by immersion alone. The part hangs or sits in the tank, the bath wets the surface and lifts the soil, and a rinse carries it away. There is no rectifier, no electrical contact and nothing to set beyond concentration and temperature, which makes these the simplest of the plating chemicals to run on a line that already has enough variables to watch.
The electrolytic types add current to the same job. Gas evolved at the part scrubs the surface while the bath works, so soil lifts out of blind holes, threads and recessed areas that a still bath struggles to reach, and the cycle shortens as a result. Results depend on clean racking and firm contact points; a part that is poorly contacted degreases unevenly. Within metal electroplating, this is often the step that decides whether a recessed part plates bright or shows a shadow.
In practice the difference comes down to geometry and volume. Open shapes with light oil run well as immersion work. Complex parts, tight recesses and high throughput justify the rectifier. Aluminum and zinc-aluminum components are handled by the lower-concentration electrolytic grade, so the bath cleans the surface without working on the substrate underneath.
| Product | Typical role |
| Brightener for SZ-30B sulfate zinc plating | Brightener for sulfate acid zinc baths |
| Bright zinc alkaline ZN 50 | Alkaline zinc process for rack and barrel lines |
| Brightener for cyanide-free alkaline zinc plating ZN-500 | Brightener for cyanide-free alkaline zinc systems |
| Phoenix EB 204A-204B | Divalent tin salt electrolytic colouring additive for aluminum |
| Phoenix Seal 149-L | Middle-temperature sealing agent for aluminum anodizing |
| Phoenix Seal 149-T | Medium-temperature sealing agent |
| FI-970 bright acid copper | High-deposit-brightness copper process for decorative metal electroplating |
| Wood, stone and concrete nano-protective FF-4219 | Nano protective treatment for non-metal surfaces |
| Nickel Purify P3 | Purifying additive for nickel baths |
| Chrome mist inhibitor FF-116 | Mist suppression for chrome plating lines |

Choosing the right match is where most sourcing decisions stall. As a trading supplier, we keep one point of contact from first enquiry to after-sales: tell us what you are making and the conditions you work under, and we shortlist the closest matches from our supplier network, compare specifications and arrange samples before you commit to a bulk order. If something does not behave as expected, we work with the supplying partner on the cause and a practical fix, and stay with the case until it is settled. Email, WeChat or WhatsApp enquiries get a reply within 24 hours.
Yes, and it is not a formality. A proper rinse after degreasing removes the alkaline film and the soil it has lifted; if either carries over, the deposit can patch, blister or lose adhesion. Two rinse stages with clean, moving water are normal practice, and the second one should stay clean enough that parts come out water-break free. In a well-run metal plating process the rinse is treated as part of the cleaning step, not as a gap between two tanks.
Check the concentration against the figure for your type and top up with the same powder, rather than adding a different cleaner to compensate. Skim or filter out the oil and sludge that accumulate on the surface and at the bottom, because a bath carrying its own soil load stops cleaning long before the chemical is used up. Most plating chemicals are judged on this kind of consistency, and a degreaser is no different: steady dosing and a clean tank give repeatable results, while occasional heavy dosing gives uneven ones.
That is exactly where they earn their place. The gas generated at the part during electrolytic degreasing lifts soil out of holes, threads and recessed faces that a still bath cannot flush, and the cycle is correspondingly shorter. The result depends on the part being properly racked with clean contact points; a poor contact leaves a shadow where the current did not reach. Tell us the geometry when you order and we will confirm which of the two electrolytic grades fits the substrate.
Type E is the grade for metal surfaces treated with polishing cream, and it is the one to specify when the parts come straight from the buffing wheel. Where the cream is particularly heavy or dried on, a dedicated removing-wax agent is available that shifts it faster than a general degrease. This matters because polishing cream clings harder than oil and, left on the surface, is a common cause of patchy adhesion later in the plating process.
Yes. The range is used in both batch and continuous production environments, and the grades are the same either way; what changes is how the bath is made up and replenished on the line. For a continuous installation, tell the sales contact the line speed, tank volume and the substrates you run, and the grade, the dosing routine and the pack format are confirmed against those numbers. The same production base supplies the rest of our coating production chemicals, so a line can standardise its pretreatment and its plating chemistry with one supplier.